Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
1.78 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-PSK3 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 3.20 µm/m-°C @Temperature 20.0 - 400 °C |
1.78 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3 SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads an.. |
|||
CTE, linear | 3.20 µm/m-°C @Temperature 20.0 - 200 °C |
1.78 µin/in-°F @Temperature 68.0 - 392 °F |
DIN EN 821-1 |
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3 SL 200 ST is a silicon nitride ceramic especially suitable for components exposed to mechanical stress and engine-specific applications even at elevated temperatures. It is recognized for its high s.. |
|||
CTE, linear | 3.20 µm/m-°C @Temperature 25.0 - 500 °C |
1.78 µin/in-°F @Temperature 77.0 - 932 °F |
|
COI Ceramics Nicalon™ CG SiCO Ceramic Fiber Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties .. |
|||
CTE, linear | 3.20 µm/m-°C @Temperature 25.0 - 1001 °C |
1.78 µin/in-°F @Temperature 77.0 - 1834 °F |
|
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2) Te value is 670°C. Hasselman Thermal Shock value is 800 K.Data provided by CeramTec North America. |
|||
CTE, linear | 3.20 µm/m-°C @Temperature -30.0 - 30.0 °C |
1.78 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX CRN730V PPE+PA6 (Asia Pacific) PPE+PA+GF, FR |