Polymer Property : Melt Flow = 68.1 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 68.1 g/10 min

@Load 5.00 kg,
Temperature 280 °C
68.1 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL GTX CRN730V PPE+PA6 (Asia Pacific)
PPE+PA+GF, FR