Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 68.1 g/10 min @Load 5.00 kg, Temperature 280 °C |
68.1 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX CRN730V PPE+PA6 (Asia Pacific) PPE+PA+GF, FR |