Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Lexan® PPC4704 PPC (Asia Pacific)

Category Polymer , Thermoplastic , Polyphthalate Carbonate
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® PPC4704 PPC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with biocompatibility information and should not be used for medical applications which require biocompatibility. Alternative grade HPH4704.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D 792
Water Absorption 0.19 %

@Time 86400 sec
0.19 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 67.0 MPa
9720 psi
SABIC - Japan Method
Elongation at Break 200 %
200 %
SABIC - Japan Method
Flexural Strength 95.0 MPa
13800 psi
ASTM D 790
Flexural Modulus 2.25 GPa
326 ksi
ASTM D 790
Izod Impact, Notched 5.09 J/cm

@Temperature 23.0 °C
9.54 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C

@Thickness 3.20 mm
325 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D 257
Dielectric Constant 3.3

@Frequency 50.0 - 60.0 Hz
3.3

@Frequency 50.0 - 60.0 Hz
ASTM D 150
Copyright © lookpolymers.com All Rights Reserved