Mechanical Properties Metric English Comments
Izod Impact, Notched 5.09 J/cm

@Temperature 23.0 °C
9.54 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® PPC4704 PPC (Asia Pacific)
High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..