Abatron AboCast 8-6/Abocure 8-6 Epoxy  (discontinued **)

Category Polymer , Thermoset , Epoxy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8-6/Abocure 8-6 Epoxy  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 115 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Water Absorption 0.24 %
0.24 %
in 24 hours.
Viscosity Measurement 1000
1000
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
Tensile Strength, Ultimate 49.64 MPa
7200 psi
Elongation at Break 6.8 %
6.8 %
Flexural Strength 84.81 MPa
12300 psi
Electrical Properties Metric English Comments
Electrical Resistivity 1.50e+10 ohm-cm

@Temperature 93.3 °C
1.50e+10 ohm-cm

@Temperature 200 °F
8.20e+12 ohm-cm

@Temperature 65.6 °C
8.20e+12 ohm-cm

@Temperature 150 °F
2.00e+15 ohm-cm

@Temperature 25.0 °C
2.00e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.48

@Frequency 1e+6 Hz
3.48

@Frequency 1e+6 Hz
Dissipation Factor 0.011

@Frequency 1e+6 Hz
0.011

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing time: 16 hours; Postcure: 2 hours/100°C (212°F)