Material Notes:
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Water Absorption 0.16 %

@Time 86400 sec
0.16 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 20 g/10 min

@Load 1.20 kg,
Temperature 300 °C
20 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.0 MPa
8270 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 110 %
110 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 81.0 MPa
11700 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.03 GPa
294 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
2.13 J/cm

@Temperature -30.0 °C
3.99 ft-lb/in

@Temperature -22.0 °F
ASTM D256
5.87 J/cm

@Temperature -20.0 °C
11.0 ft-lb/in

@Temperature -4.00 °F
ASTM D256
2.13 J/cm

@Thickness 6.40 mm
3.99 ft-lb/in

@Thickness 0.252 in
ASTM D256
Dart Drop, Total Energy 56.0 J
41.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 64.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
36.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 126 °C

@Thickness 6.40 mm
259 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C

@Thickness 3.20 mm
244 °F

@Thickness 0.126 in
unannealed; ASTM D648
123 °C

@Thickness 6.40 mm
253 °F

@Thickness 0.252 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C
176 °F
UL 746B
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
UL RTI, Mechanical without Impact 80.0 °C
176 °F
UL 746B
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
UL 94