Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 244 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 118 °C

@Thickness 3.20 mm
244 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Lexan® EM3110 PC
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses.
Deflection Temperature at 1.8 MPa (264 psi) 118 °C

@Thickness 3.20 mm
244 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific)
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses.
Deflection Temperature at 1.8 MPa (264 psi) 118 °C

@Thickness 3.20 mm
244 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics Lexan® EM3110R PC
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 118 °C

@Thickness 3.20 mm
244 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Lexan® EM3110R PC (Asia Pacific)
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release.
Deflection Temperature at 1.8 MPa (264 psi) 118 °C

@Thickness 6.40 mm
244 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL REN501 PPE+PS
Noryl REN501 resin is an unfilled Post Industrial Recycle (PIR) based injection moldable modified polyphenylene ether blend comprising up to 40% PIR content. Available in black only.
Deflection Temperature at 1.8 MPa (264 psi) 118 °C

@Thickness 3.20 mm
244 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL ENG265 PPE+PS
PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a..
Copyright © lookpolymers.com All Rights Reserved