Polymer Property : Dart Drop, Total Energy = 41.3 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® RCM6123 PC+ABS (Asia Pacific)
Cycoloy* RCM6123 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1..
Dart Drop, Total Energy 56.0 J
41.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® EM3110 PC
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses.
Dart Drop, Total Energy 56.0 J
41.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific)
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses.
Dart Drop, Total Energy 56.0 J
41.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics Lexan® EM3110R PC (Asia Pacific)
Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. Internal mold release.
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific)
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East)
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific)
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Europe-Africa-Middle East)
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
Dart Drop, Total Energy 56.0 J
41.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC
LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121.
Dart Drop, Total Energy 56.0 J
41.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Asia Pacific)
Alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121.
Dart Drop, Total Energy 56.0 J

@Temperature -30.0 °C
41.3 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics ULTEM 8015 PEI
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 100/100 with low toxicity, smoke, and flame evolution. ECO Conforming.
Dart Drop, Total Energy 56.0 J

@Temperature -30.0 °C
41.3 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics ULTEM 8015 PEI (Asia Pacific)
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 100/100 with low toxicity, smoke, and flame evolution. ECO Conforming.
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® 6620U PBT+PC
PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance.
Dart Drop, Total Energy 56.0 J
41.3 ft-lb
ASTM Test
Styrolution Luran® S 777 K ASA
Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance.
Dart Drop, Total Energy 56.0 J
41.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66
LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact.
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® FXV310SK PBT
VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances.
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer
Dart Drop, Total Energy 56.0 J

@Temperature 23.0 °C
41.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer
Dart Drop, Total Energy 56.0 J
41.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 (Asia Pacific)
LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact.