SABIC Innovative Plastics LNP THERMOTUF VF008 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF VF008 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP THERMOTUF* VF008 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Moisture Absorption 0.500 %
0.500 %
50% RH, 24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 131 MPa
19000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 9.64 GPa
1400 ksi
ASTM D790
Izod Impact, Notched 1.92 J/cm
3.60 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.91 J/cm
16.7 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 32.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Thermal Conductivity 0.380 W/m-K
2.64 BTU-in/hr-ft²-°F
ASTM E 1530
Deflection Temperature at 1.8 MPa (264 psi) 245 °C

@Thickness 3.20 mm
473 °F

@Thickness 0.126 in
unannealed; ASTM D648