Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 500 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 500R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 503R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL910 PC Various weight reductions at 0.250"" (6.35 mm) wall, 10% GR. High flexural strength and modulus, impact/heat resistant. V-0/5V at 0.250"" (6.35 mm). |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2100F PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing, WRAS certification in recognized colors.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 2100N PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 2100N PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PC 04008 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M19 HS BK 19% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 19% Filler by Weight and Mineral Filler, 19% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M20 IM BK 20% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight and Mineral Filler, 20% Filler by WeightAdditive: Lubricant, Impact Modifier and Heat S.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF13 HS L BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF13 L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF13 X BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF14 HS L BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF15 L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF15 TL5 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: PTFE Lubricant (5%)Features: LubricatedAppearance: Natural ColorInformation p.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated TPCI# 8263101Information provided by TP Composit.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF35 HS L 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and heat StabilizedProcessin.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF13 SL2 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and Silicone LubricantFeatures: Lubricated and Heat StabilizedInformation pr.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PC GF20 TL10 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, In.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF VF008 PA 66 (Asia Pacific) LNP THERMOTUF* VF008 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT GF15 BK001 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: BlackTPCI# 6100111Information provided by TP Composit.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT GF15 RD 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: RedTPCI# 862111Information provided by TP Composites,.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PES GM20 WT139 20% Milled Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |