Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 503 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 503R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL913 PC Various weight reduction at 0.250"" (6.35 mm) wall. 10% GR, high flexural strength/modulus. UL rated V-0/5VA (all except natural). UV-stabilized. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL410 PC Various weight reductions at 0.250: (6.38 mm) wall. Thin wall capability high flexural mod, strength and creep resistant. V-0/5V - 0.157""(3.98 mm). |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2100F PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing. WRAS certification in recognized col.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 2100N PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2100R PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2100R PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PC 04008 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PC GF10 FR BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightFeatures: Flame Retardant Appearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF/M19 HS BK 19% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 19% Filler by Weight and Mineral Filler, 19% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF13 L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF13 TL10 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: PTFE Lubricant (10%)Features: LubricatedAppearance: Natural ColorInformation .. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF14 HS L BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF15 TL5 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: PTFE Lubricant (5%)Features: LubricatedAppearance: Natural ColorInformation p.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF30 HS L BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 HR HS BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Hydrolysis Resistant Appearance: .. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedProcessin.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated TPCI# 8263101Information provided by TP Composit.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF35 L UV 35% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PC GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PES GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF13 ML2 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Heat Stabiliz.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PC GF20 TL10 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, In.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PPS/F 0328 Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |