Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7604 PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7604 PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Water Absorption 0.12 %

@Time 86400 sec
0.12 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0030 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.0 MPa
13900 psi
SABIC - Japan Method
Elongation at Break 4.0 - 6.0 %
4.0 - 6.0 %
SABIC - Japan Method
Flexural Strength 132 MPa
19100 psi
ASTM D790
Flexural Modulus 5.49 GPa
796 ksi
ASTM D790
Izod Impact, Notched 0.780 J/cm
1.46 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 - 55.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 30.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 100 °C

@Thickness 3.20 mm
212 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Users viewing this material also viewed the following: