Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC LNP LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | SABIC - Japan Method |
SABIC Innovative Plastics Lexan® SP7604 PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | ISO 527-1/-2 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 8015 PEI High flow Polyetherimide blend. Meets FAR 25.853 and OSU 100/100 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 8015 PEI (Asia Pacific) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 100/100 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp ZFL34 PPO LNP* Lubricomp* ZFL34 is a compound based on Modified PPO containing glass fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM ATX200R PEI+PCE (Asia Pacific) High flow Polyetherimide blend with internal mold release. ECO Conforming. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem AUT230M PEI (Asia Pacific) Transparent polyetherimide (Tg 247 degC) with internal mold release. Very low outgassing and plateout for automotive lighting applications where highly metallized, reflective surfaces are required... |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific) Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem UR9076LG PEI Standard flow mineral filled Polyetherimide Blend. Restricted sales to GE Specialty Film & Sheet.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type 1A, 50 mm/min; ISO 527-2 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | SABIC - Japan Method |
SABIC Innovative Plastics Valox® VIC4311 PBT (Asia Pacific) |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+HIPS (Europe-Africa-Middle East) DATA ON BK1005 ONLY. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM AUT230 PEI Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | ASTM D638 |
Cresset Powers Cress-Alon™ NE2740 4% Nano Clay Loaded, 2.7 r.v. Compounding Grade Nylon 6, 50% RH Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Strength, Yield | 96.0 MPa | 13900 psi | 50 mm/min; ISO 527-2 |
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, .. |