SABIC Innovative Plastics LNP THERMOCOMP HF004 PA 11

Category Polymer , Thermoplastic , Nylon , Nylon 11
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP HF004 PA 11.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* HF004 is a compound based on Nylon 11 resin containing 20% Glass Fiber.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 81.0 MPa
11700 psi
ISO 527
Elongation at Break 12.2 %
12.2 %
ISO 527
Tensile Modulus 3.67 GPa
532 ksi
1 mm/min; ISO 527
Flexural Strength 100 MPa
14500 psi
ISO 178
Flexural Modulus 3.54 GPa
513 ksi
ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af