Material Notes:
Molecular Formula: NH4BrCas No.: 12124-97-9Mainly used as sensitization film, photograph mulsion material, photographic paper and medicine, plastic, printing agents, etc.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
pH 4.5 - 6.0
4.5 - 6.0
0.05
Optical Properties Metric English Comments
Transmission, Visible 93 - 100 %

@Wavelength 410 nm
93 - 100 %

@Wavelength 410 nm
Solution (250g/l)
Component Elements Properties Metric English Comments
Bismuth, Bi <= 0.000020 %
<= 0.000020 %
Copper, Cu <= 0.000050 %
<= 0.000050 %
Iron, Fe <= 0.000050 %
<= 0.000050 %
Lead, Pb <= 0.000020 %
<= 0.000020 %
Descriptive Properties Value Comments
Appearance White crystal
CAS Number 12124-97-9
Chloride (%) <0.2
Color Solution (250g/l) <15.0
Content (%) >99.5
Insoluble (%) <0.005
Water insolubles
Iodide (%) <0.001
Loss on Drying (%) <0.5
Molecular Formula NH4Br
Sulphate (%) <0.005
Transparency Qualified