SABIC Innovative Plastics LNP THERMOCOMP 5C004 PVDF (Asia Pacific)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP 5C004 PVDF (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* 5C004 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 84.0 MPa
12200 psi
ASTM D638
Elongation at Break 0.70 %
0.70 %
ASTM D638
Tensile Modulus 16.44 GPa
2384 ksi
50 mm/min; ASTM D638
Flexural Strength 137 MPa
19900 psi
ASTM D790
Flexural Modulus 13.93 GPa
2020 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.85 J/cm
5.34 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 153 °C

@Thickness 3.20 mm
307 °F

@Thickness 0.126 in
unannealed; ASTM D648