SABIC Innovative Plastics LNP Stat-kon DS0029 PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Stat-kon DS0029 PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* DS0029 is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.0 MPa
7110 psi
ASTM D 638
Tensile Strength, Yield 57.0 MPa
8270 psi
ASTM D 638
Elongation at Break 7.8 %
7.8 %
ASTM D 638
Elongation at Yield 4.3 %
4.3 %
ASTM D 638
Flexural Strength 96.0 MPa
13900 psi
ASTM D 790
Flexural Modulus 2.90 GPa
421 ksi
ASTM D 790
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 13.35 J/cm

@Temperature 23.0 °C
25.01 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C

@Thickness 3.20 mm
124 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Electrical Properties Metric English Comments
Surface Resistance 10000 - 1.00e+6 ohm
10000 - 1.00e+6 ohm
ASTM D 257