Goodfellow T1-Thermocouple Alloy

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow T1-Thermocouple Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The positive element of the type K thermocouple alloy the negative being T2. The thermocouple can be used up to 1250C in oxidizing atmospheres and is the probably the most common in use. It is also the positive element of the type E thermocouple with Constantan as the negative; the thermoelectric power of type E thermocouples is the highest amongst all standard couplesInformation provided by Goodfellow.
Physical Properties Metric English Comments
Density 8.50 g/cc
0.307 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 620 - 780 MPa
89900 - 113000 psi
Elongation at Break <= 44 %
<= 44 %
Modulus of Elasticity 186 GPa
27000 ksi
Izod Impact, Unnotched 1.08 J/cm
2.02 ft-lb/in
Notch Status Unknown
Thermal Properties Metric English Comments
CTE, linear 17.2 µm/m-°C

@Temperature 20.0 - 1000 °C
9.56 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 19.0 W/m-K
132 BTU-in/hr-ft²-°F
Melting Point 1420 °C
2590 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Component Elements Properties Metric English Comments
Chromium, Cr 10 %
10 %
Nickel, Ni 90 %
90 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000706 ohm-cm
0.0000706 ohm-cm
Temperature Coefficient of 0.00032/K