SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Moisture Absorption 0.280 %
0.280 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 52.7 %
52.7 %
ASTM D638
Flexural Strength 54.0 MPa
7830 psi
ASTM D790
Flexural Modulus 1.72 GPa
249 ksi
ASTM D790
Izod Impact, Notched 6.03 J/cm
11.3 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 117 µm/m-°C

@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C

@Thickness 3.20 mm
131 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 10000 ohm-cm
100 - 10000 ohm-cm
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257