Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON EX99550C PEI

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON EX99550C PEI.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* STAT-KON* EX99550C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Moisture Absorption 0.210 %
0.210 %
50% RH, 24 hrs; ASTM D570
0.320 %
0.320 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Time 86400 sec
0.0010 in/in

@Time 24.0 hour
ASTM D955
0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
0.0034 cm/cm

@Time 86400 sec
0.0034 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 149 MPa
21600 psi
ISO 527
189 MPa
27400 psi
ASTM D638
Elongation at Break 0.70 %
0.70 %
ISO 527
1.1 %
1.1 %
ASTM D638
Tensile Modulus 20.68 GPa
2999 ksi
50 mm/min; ASTM D638
22.94 GPa
3327 ksi
1 mm/min; ISO 527
Flexural Strength 251 MPa
36400 psi
ISO 178
266 MPa
38600 psi
ASTM D790
Flexural Modulus 18.68 GPa
2709 ksi
ISO 178
18.76 GPa
2721 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.52 J/cm
6.59 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 J
5.90 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
18.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 21.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
21.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
201 °C

@Thickness 3.20 mm
394 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 0.350 mm
V-0

@Thickness 0.0138 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 1.0 - 10000 ohm
1.0 - 10000 ohm
ASTM D257