Polymer Property : Linear Mold Shrinkage, Flow = 0.0015 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched
LNP* LUBRICOMP* OCP36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific)
LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive..
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0015 - 0.0018 cm/cm

@Thickness 2.00 mm
0.0015 - 0.0018 in/in

@Thickness 0.0787 in
Solvay Specialty Polymers Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® FC-1150 is an FDA-approved, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DF006P PC
LNP THERMOCOMP* DF006P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing.
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP TF006 PU
LNP THERMOCOMP TF006 is a compound based on Polyurethane containing 30% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP QFL17RS PA 6/10
LNP LUBRICOMP* QFL17RS is a compound based on Nylon 6/10 resin containing 35% Glass Fiber, 5% PTFE. Added features of this material include: Easy Release, Heat Stabilized, Wear Resistant.
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Stat-kon DX96690 PC
LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America..
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Time 86400 sec
0.0015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON EX99550C PEI
LNP* STAT-KON* EX99550C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.