Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 20.68 GPa | 2999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Tensile Modulus | 20.68 GPa | 2999 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Tensile Modulus | 20.68 GPa | 2999 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Tensile Modulus | 20.68 GPa | 2999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
Tensile Modulus | 20.68 GPa | 2999 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON EX99550C PEI LNP* STAT-KON* EX99550C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |