Mechanical Properties Metric English Comments
Tensile Modulus 22.94 GPa
3327 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON EX99550C PEI
LNP* STAT-KON* EX99550C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.