Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Internally lubricated Polyphthalamide compound, containing Carbon Fiber and PTFE. Added features include Heat Stabilized
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 272 MPa
39500 psi
5 mm/min; ISO 527
Elongation at Break 1.4 %
1.4 %
5 mm/min; ISO 527
Tensile Modulus 21.8 GPa
3160 ksi
1 mm/min; ISO 527
Flexural Yield Strength 373 MPa
54100 psi
2 mm/min; ISO 178
Flexural Modulus 19.0 GPa
2760 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 7.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
3.89 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 46.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
25.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2