Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 373 MPa | 54100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, containing Carbon Fiber and PTFE. Added features include Heat Stabilized |