Polymer Property : Tensile Modulus = 21.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 21.8 GPa
3160 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East)
Internally lubricated Polyphthalamide compound, containing Carbon Fiber and PTFE. Added features include Heat Stabilized
Tensile Modulus 21.8 GPa
3160 ksi
ISO 527
Azoty Tarnow™ Tarnamid® T-27 CF40 Polyamide 6 40% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..