Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 272 MPa | 39500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, containing Carbon Fiber and PTFE. Added features include Heat Stabilized |
|||
Tensile Strength at Break | 272 MPa | 39500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EC006PXQ PEI LNP* THERMOCOMP* EC006PXQ is a compound based on Polyetherimide containing 30% Carbon FIber. Added features include: Electrically Conductive, Easy Molding. |
|||
Tensile Strength at Break | 272 MPa | 39500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EC008PXQ PEI LNP* THERMOCOMP* EC008PXQ is a compound based on Polyetherimide containing 40% Carbon FIber. Added features include: Electrically Conductive, Exceptional Processing |