SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA 12 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA 12 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conductive.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 124 MPa
18000 psi
ASTM D638
Elongation at Break 2.7 %
2.7 %
ASTM D638
Tensile Modulus 15.72 GPa
2280 ksi
50 mm/min; ASTM D638
Flexural Strength 206 MPa
29900 psi
ASTM D790
Flexural Modulus 13.85 GPa
2009 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.94 J/cm
13.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 168 °C

@Thickness 3.20 mm
334 °F

@Thickness 0.126 in
unannealed; ASTM D648