Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.72 GPa | 2280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA 12 (Asia Pacific) LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conductive. |