Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP AL001 ABS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP AL001 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* AL-4010 HP is a compound based on Acrylonitrile Butadiene Styrene resin containing 5% PTFE. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.0 MPa
5660 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 69.0 MPa
10000 psi
ASTM D790
Flexural Modulus 2.46 GPa
357 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.89 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm
11.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C

@Thickness 3.20 mm
176 °F

@Thickness 0.126 in
unannealed; ASTM D648
Copyright © lookpolymers.com All Rights Reserved