Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790-92 |
Multibase Multi-Pro® 2012 RC 20% Glass Filled Polypropylene Moisture content is 0.06%. Multi-Pro 2012 RC is a glass reinforced polypropylene, chemically coupled which enhances the mechanical properties. This product has been formulated to achieve an esthe.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 2 mm/min; ISO 178 |
Polimeri Europa Edistir N 1840 Polystyrene General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Polimeri Europa Sinkral® PD L 322 ABS Resin Sinkral PD L 322 by continuous mass, is a general purpose, high flow injection molding grade having good impact resistance coupled with an excellent gloss.Applications: Widely used in the small and.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific) Thermally conductive electrically insulative mineral filled PPS FR compound. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | |
Poco Graphite AXM-5Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips MC3200 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical partsConsumer containers, vials, jars, etc.Clock lensesAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat softening tempera.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 0.1 in/min; ASTM D790 |
Ineos Nova 879 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High heat crystal polystyrene, Color stable, Custom colorsApplications: Injection molding, Designed for applications requiring high strength, high heat resistance, and color stabilityPerformance gra.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
LG Chemical HI855H PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp DP0039 PC LNP* Lubricomp* DP0039 is a Polycarbonate base resin containing PTFE and Silicone lubricants. Characteristics are: Flame Retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ISO 178 |
SABIC Innovative Plastics LNP Lubricomp KI001A Acetal LNP* Lubricomp Fulton 441D is an Acetal based compound with Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10 LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Strength | 69.0 MPa | 10000 psi | |
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | |
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | at rupture; ASTM D790 |
Sumitomo Bakelite North America RX® 525 Cellulose Reinforced Phenolic Novolac RX 525 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for parts requiring moderate toughness. It is designed to meet the requirements of ASTM D-594.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | |
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | at rupture; ASTM D790 |
Sumitomo Bakelite North America SI 9041A Silicone Compound SI 9041A is a long fiberglass reinforced silicone molding compound, which exhibits excellent high temperature properties in addition to good molding characteristics for transfer and compression mold.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Plenco 7200 Phenolic, Granular, Injection Molded PLENCO 07200 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength, good powder properties and excellent cosmetic properties. UL recognized under component .. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Eastman Aspira EN177 Copolyester Resin for Extrusion Blow Molding Applications:Beverage packagingConsumer packagingFood packagingPersonal care packagingKey Attributes:BPA-freeCompatible with high-output manufacturing platformsExcellent clarityHigh gloss appearance.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 500 GB6 POM 30% glass beads filled low viscosity grade with very high stiffness and hardness with lowered shrinkage combined with easy molding of complicated shapesInformation provided by Zakłady Azotowe w .. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 700 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® 220Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Ashley Polymers Ashlene® ABS Resin F-216 General purpose high impact resin.Data provided by the manufacturer |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM Test |
BASF Ultramid® HPN 9350 HS PA6 (Dry) Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 604 Nylon 6/6, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Flexural Strength | 69.0 MPa | 10000 psi | ASTM D790 |
Resinoid 2010 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |