SABIC Innovative Plastics LNP COLORCOMP R1000SU PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Colorcomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP COLORCOMP R1000SU PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP COLORCOMP* R1000SU is an unfilled Nylon 66 resin. Added features include: Heat Stabilized, UV Stabilized.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
1.23 g/cc
0.0444 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Tensile Modulus 3.40 GPa
493 ksi
1 mm/min; ISO 527
Flexural Strength 11.0 MPa
1600 psi
ISO 178
Flexural Modulus 3.20 GPa
464 ksi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af