Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.40 GPa | 493 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS (Asia Pacific) PC/ABS with high stiffness and impact performance |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data) Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1,2 |
Qualchem Danamid FEW-25 Polyamide 6, 25% Mineral Filled Filled with mineralsInformation provided by Qualchem Zrt. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 7425 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, low tendency to warp, improved surface finish |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | |
LATI Laticonther 52/35 CP1/45 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 LNP* LUBRICOMP* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
Solvay Specialty Polymers Ryton® QA200P Polyphenylene Sulfide (PPS) Ryton® QA200P (pelletized) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and may be used in injection molding processes.Features: Good Chemical Resis.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
Solvay Specialty Polymers Ryton® QC160P Polyphenylene Sulfide (PPS) Ryton® QC160P (pelletized) polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Chemical Resista.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP ZX08005 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZX08005 is a Compound based on PPE + PS Blend resin, containing Mineral. Added features include: Improved Dielectric Properties. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 |
Westlake Plastics MediPEEK IM Polyetheretherketone for Medical Applications MediPEEK-IM is a high performance semi-crystalline thermoplastic designed for long term body contact as an implantable material. It is USP Class VI and compliant to ASTM F2026. It has excellent st.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-15 S PA6-GF15 Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MR 409 HWCP Mineral Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TS350 PA46 FR(17) Unreinforced, Flame Retardant |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 HWS Nylon 66, Finely Crystalline, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Tensile Modulus | 3.40 GPa | 494 ksi | Storage |
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam P10002Z PA6, Flame Retardant, Extrusion Starflam P10002Z is an Unfilled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Extrusion ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam PX06091 PA6, Flame Retardant, Injection Molded Starflam PX06091 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam BFR200Y PA6, Flame Retardant, Injection Molded Starflam BFR200Y is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2/1A/1 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (5 mi.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
CENTROPLAST CENTRO HPM Polyetherimide This material has high strength and rigidity at high temperatures, with good electrical properties. Applications include electrical insulators, and load-bearing components.Information provided by C.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 23.0 °C |
493 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |