Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cycoloy* C7210A resin is talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 16.4 g/10 min

@Load 2.16 kg,
Temperature 260 °C
16.4 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.0 MPa
6960 psi
Type I, 5 mm/min; ASTM D638
Tensile Strength, Yield 63.0 MPa
9140 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 80 %
80 %
Type I, 5 mm/min; ASTM D638
Elongation at Yield 3.6 %
3.6 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 3.51 GPa
509 ksi
5 mm/min; ASTM D638
Flexural Strength 106 MPa
15400 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.14 GPa
455 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256
Izod Impact, Unnotched 18.69 J/cm
35.01 ft-lb/in
ASTM D4812
Dart Drop, Total Energy 47.0 J

@Temperature 23.0 °C
34.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 59.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 66.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C

@Thickness 3.20 mm
198 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C

@Thickness 3.20 mm
180 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 101 °C
214 °F
Rate B/50; ASTM D1525
UL RTI, Electrical 60.0 °C
140 °F
UL 746B
UL RTI, Mechanical with Impact 60.0 °C
140 °F
UL 746B
UL RTI, Mechanical without Impact 60.0 °C
140 °F
UL 746B
Flammability, UL94 V-0

@Thickness 1.19 mm
V-0

@Thickness 0.0469 in
UL 94
5VB

@Thickness 1.98 mm
5VB

@Thickness 0.0780 in
UL 94
Users viewing this material also viewed the following: