Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 18.69 J/cm | 35.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific) Cycoloy* C7210A resin is talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
Izod Impact, Unnotched | 18.69 J/cm | 35.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific) LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 18.69 J/cm | 35.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
Izod Impact, Unnotched | 18.69 J/cm @Temperature 23.0 °C |
35.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl N190HX PPE+PS High gloss. 182F (83C) HDT. UL94 V-0/5VA rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 18.69 J/cm @Temperature 23.0 °C |
35.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp Cycoloy_C7210A PC+ABS (Asia Pacific) Talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.This data was supplied by SABIC-IP for the Asia Pacific region. |