Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 16.4 g/10 min @Load 2.16 kg, Temperature 260 °C |
16.4 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific) Cycoloy* C7210A resin is talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
Melt Flow | 16.4 g/10 min @Load 2.16 kg, Temperature 260 °C |
16.4 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
Melt Flow | 16.4 g/10 min @Load 2.16 kg, Temperature 260 °C |
16.4 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics LNP Thermocomp Cycoloy_C7210A PC+ABS (Asia Pacific) Talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.This data was supplied by SABIC-IP for the Asia Pacific region. |