Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.14 GPa | 455 ksi | ASTM D790 |
Oxford Polymers C-Acetal 10MF-900 BK Acetal Product Description: Acetal Injection Molding Grade, 10 melt flow Processing and Delivery Form: Pellets and Injection MoldingSpecial Characteristics: Pre-colored blackInformation provided by Oxford.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific) Cycoloy* C7210A resin is talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | ASTM Data |
BASF Capron® 5202 HS Blend Nylon 66 (Dry)
(discontinued **) Capron 5202 HS Blend is a blended, unfilled, heat stabilized, nylon 6,6, injection molding compound. It is also available in natural and pigmented versions. It combines strength and stiffness as wel.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | ASTM D790 |
I. Stern N1841 General Purpose Crystal Polystyrene Features:Excellent Process PropertiesEasy FlowApplicationsDisplaysToys, CosmeticsAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. Stern & Co. Inc. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | ASTM D790 |
I. Stern N2380 High Heat Crystal Polystyrene Features:High Molecular WeightExcellent Optical PropertiesApplicationsOPSFoamed TraysThick Walled Injection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | ASTM D790 |
Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN3322VO Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Modulus | 3.14 GPa @Thickness 6.40 mm |
455 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL GP3302 PP+MF30% Description: Injection Molding, PP+MF30%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | DIN 53452; ASTM D790 |
Kolon NOPLA® KE531HC PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Flexural Modulus | 3.14 GPa @Thickness 3.20 mm |
455 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY EC5000A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | ASTM D790 |
Samyang Trirex® 3025GN10 Polycarbonate, Reinforced Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025GN10 is a reinforced flame retardant grade.Applications: LCD Panel Frame (dimensio.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM AUT210 PEI Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Europe-Africa-Middle East) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp Cycoloy_C7210A PC+ABS (Asia Pacific) Talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | ASTM D790 |
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | ASTM D790 |
Tipco Tipcolene® CR 6216 - 40% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology 40% Mineral Reinforced, Controlled Rheology PP CopolymerApplications: Automotive Air DuctsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | ASTM D790 |
Tipco Tipcolene® SEB 100 - 10% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability 10% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 3.14 GPa @Temperature 177 °C |
455 ksi @Temperature 350 °F |
Resin property; Dry |
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l.. |
|||
Flexural Modulus | >= 3.14 GPa | >= 456 ksi | ASTM D790 |
Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 250 uses a higher fiberglass/PTFE ratio to provide mechanical properties approaching those of conventional substrates. Better dimensional stability and lower thermal expansion in all directi.. |
|||
Flexural Modulus | 3.14 GPa | 455 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973. |