Polymer Property : Flexural Modulus = 455 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.14 GPa
455 ksi
ASTM D790
Oxford Polymers C-Acetal 10MF-900 BK Acetal
Product Description: Acetal Injection Molding Grade, 10 melt flow Processing and Delivery Form: Pellets and Injection MoldingSpecial Characteristics: Pre-colored blackInformation provided by Oxford..
Flexural Modulus 3.14 GPa
455 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific)
Cycoloy* C7210A resin is talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.
Flexural Modulus 3.14 GPa
455 ksi
ASTM Data
BASF Capron® 5202 HS Blend Nylon 66 (Dry)  (discontinued **)
Capron 5202 HS Blend is a blended, unfilled, heat stabilized, nylon 6,6, injection molding compound. It is also available in natural and pigmented versions. It combines strength and stiffness as wel..
Flexural Modulus 3.14 GPa
455 ksi
ASTM D790
I. Stern N1841 General Purpose Crystal Polystyrene
Features:Excellent Process PropertiesEasy FlowApplicationsDisplaysToys, CosmeticsAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. Stern & Co. Inc.
Flexural Modulus 3.14 GPa
455 ksi
ASTM D790
I. Stern N2380 High Heat Crystal Polystyrene
Features:High Molecular WeightExcellent Optical PropertiesApplicationsOPSFoamed TraysThick Walled Injection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St..
Flexural Modulus 3.14 GPa
455 ksi
ASTM D790
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Flexural Modulus 3.14 GPa
455 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN3322VO Flame Retardant Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Flexural Modulus 3.14 GPa

@Thickness 6.40 mm
455 ksi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL GP3302 PP+MF30%
Description: Injection Molding, PP+MF30%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG..
Flexural Modulus 3.14 GPa
455 ksi
DIN 53452; ASTM D790
Kolon NOPLA® KE531HC PEN-PET Copolyester
NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac..
Flexural Modulus 3.14 GPa

@Thickness 3.20 mm
455 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY EC5000A PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical
Flexural Modulus 3.14 GPa
455 ksi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI
LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant.
Flexural Modulus 3.14 GPa
455 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC
LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable.
Flexural Modulus 3.14 GPa
455 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS
LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.
Flexural Modulus 3.14 GPa
455 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled
Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries.
Flexural Modulus 3.14 GPa
455 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled
Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries.
Flexural Modulus 3.14 GPa
455 ksi
ASTM D790
Samyang Trirex® 3025GN10 Polycarbonate, Reinforced Flame Retardancy
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025GN10 is a reinforced flame retardant grade.Applications: LCD Panel Frame (dimensio..
Flexural Modulus 3.14 GPa
455 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics ULTEM AUT210 PEI
Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti..
Flexural Modulus 3.14 GPa
455 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific)
Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o..
Flexural Modulus 3.14 GPa
455 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics ULTEM AUT210 PEI (Europe-Africa-Middle East)
Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o..
Flexural Modulus 3.14 GPa
455 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp Cycoloy_C7210A PC+ABS (Asia Pacific)
Talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 3.14 GPa
455 ksi
ASTM D790
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated
Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor..
Flexural Modulus 3.14 GPa
455 ksi
ASTM D790
Tipco Tipcolene® CR 6216 - 40% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology
40% Mineral Reinforced, Controlled Rheology PP CopolymerApplications: Automotive Air DuctsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Modulus 3.14 GPa
455 ksi
ASTM D790
Tipco Tipcolene® SEB 100 - 10% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability
10% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Flexural Modulus 3.14 GPa

@Temperature 177 °C
455 ksi

@Temperature 350 °F
Resin property; Dry
Hexcel® HexFlow® RTM651 One-part Modified BMI Resin
HexFlow® RTM651 is a one-component modified bismaleimide for resin transfer molding (RTM). Upon heating to 212-248°F, the resin will become a low viscosity homogeneous liquid that has a long pot-l..
Flexural Modulus 3.14 GPa
455 ksi
2 mm/min, 64mm span; ISO 178
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP
SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973.