Material Notes:
REPOL Polypropylene B550MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol B550MN is recommended for use in injection molding processes where high flow and medium impact strength are required. It is an ideal material for appliance parts, automotive compounds, grilled and thin wall products. Repol B550MN contains nucleating agent.Features:Excellent flow characteristicsShort molding cycle Consistent processabilityGood stiffness-impact balanceGood surface glossInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 55 g/10 min

@Load 2.16 kg,
Temperature 230 °C
55 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
50mm/min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
50mm/min; ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648