Reliance Industries Relene W43006 Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Reliance Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Relene W43006 Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Relene W43006 is a polyethylene grade recommended for insulation in jelly filled telecommunication cables. This grade contains a special stabilization system for improved thermal resistance. It is designed to provide excellent processability for high speed wire insulating extrusion process, resistance to petroleum jelly absorption, environmental stress cracking resistance and desired electrical insulation properties. Information provided by Reliance Industries
Physical Properties Metric English Comments
Density 0.943 g/cc
0.0341 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
F<sub>0</sub>; ASTM D1693/B
Oxidative Induction Time (OIT) >= 70 min
>= 70 min
ASTM D3895
Melt Flow 0.60 g/10 min

@Load 2.16 kg
0.60 g/10 min

@Load 4.76 lb
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.5 MPa
2680 psi
ASTM D638
Elongation at Break 480 %
480 %
ASTM D638
Flexural Modulus 0.600 GPa
87.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Softening Point 118 °C
244 °F
ASTM D1525
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 2.3
2.3
ASTM D150
Dissipation Factor 0.000040
0.000040
ASTM D150