Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N2233HL BK Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Filled, Impact Grade
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N2233HL BK Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Processing Method: Injection Molding Color: BlackInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Water Absorption 1.1 %

@Time 86400 sec
1.1 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 121
121
ASTM D785
Tensile Strength at Break 141 MPa
20500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 8.62 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Copyright © lookpolymers.com All Rights Reserved