Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N1200HL BK Nylon 6/6  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1200HL BK Nylon 6/6  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North AmericaAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedAuto Specifications: DELPHI QMPL-1257 Color: BlackForm: PelletsInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 0.90 %

@Time 86400 sec
0.90 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ASTM D955 and ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Tensile Strength at Break 75.8 MPa
11000 psi
ASTM D638
75.8 MPa
11000 psi
ISO 527-2
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
97.2 MPa
14100 psi
ISO 178
Flexural Modulus 2.83 GPa
410 ksi
ASTM D790
2.83 GPa
410 ksi
ISO 178
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 48.3 kJ/m²
23.0 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 238 °C
460 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: