Material Notes:
Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and operated at medium to high ambient temperatures. It is also ideal for use as a fifth wheel grease commonly found on tractor/trailers. The No. 1 grade provides better fluidity and is recommended for lower ambient temperatures. Tacna 2000 is manufactured from high-viscosity index paraffinic base oils and lithium 12-hydroxy stearate soap stock. It is fortified with an adhesive polymer, rust and corrosion inhibitors, and an effective extreme-pressure additive, which results in an exceptionally stable grease that resists separation under heavy loads. It is also extremely resistant to water washing, as evidenced by its excellent water-washout and spray-off characteristics. Tacna 2000 contains an effective polymer which prevents oil bleeding while providing an exceptional level of protection under shock loading conditions.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Viscosity Measurement 95
95
Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 880 SUS
880 SUS
Base Oil Property
Saybolt Viscosity at 210°F 86 SUS
86 SUS
Base Oil Property
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil
Kinematic Viscosity at 100°C (212°F) 14 cSt
14 cSt
Base Oil
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
Four Ball Wear 0.480 mm
0.0189 in
Penetration 266 - 294
266 - 294
Worked 10,000 strokes
Penetration P(60), 1/10 mm 280
280
Timken Test 22700 g
50.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Pour Point -12.2 °C
10.0 °F
(Base Oil Property)
Dropping Point 204 °C
400 °F
Descriptive Properties Value Comments
ASTM Rust Test (A & B) Pass
Color Amber
Copper Corrosion 3A
Low Temperature Mobility 0.1 gm/sec
at 0°F
0.4 gm/sec
at 10°F
1 gm/sec
at 20°F
Oxidation Stability 3 psi drop/100 hrs
7 psi drop/500 hrs
Roll Stability 1% Change
Soap Type (Thickener) Lithium
Water Spray Off 5 wt.% Loss
Water Washout 5 wt.% Loss
175°F