Automotive cooling liquid resistant PA66-GF30 grade designed to resist even in more severe operating condition. Indicated as "top of the class" material.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Water Absorption 1.7 %
1.7 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 175 MPa
25400 psi
ISO 527
Elongation at Break 3.0 %
3.0 %
ISO 527
Tensile Modulus 9.70 GPa
1410 ksi
ISO 527
Flexural Modulus 8.60 GPa
1250 ksi
ISO 178
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75
Flammability, UL94 HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in