Pyrotek Hirolex HG Electrical Insulating Material

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name Hirolex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Hirolex HG Electrical Insulating Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hirolex HG has superior mechanical properties. It is highly resistant to thermal shock, non-flammable and offers good arc resistance.Information provided by Pyrotek.
Physical Properties Metric English Comments
Specific Gravity 1.95 g/cc
1.95 g/cc
Water Absorption 0.50 %
0.50 %
Mechanical Properties Metric English Comments
Flexural Strength 303 MPa
43900 psi
Compressive Strength 379 MPa
55000 psi
Izod Impact, Notched 16.0 J/cm
30.0 ft-lb/in
Thermal Properties Metric English Comments
Thermal Conductivity 0.360 W/m-K
2.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 250 °C
482 °F
Continuous use
510 °C
950 °F
Flammability, UL94 V-0
V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 10.0 kV/mm
254 kV/in
Arc Resistance 260 sec
260 sec