Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | |
Pyrotek Hirolex HG Electrical Insulating Material Hirolex HG has superior mechanical properties. It is highly resistant to thermal shock, non-flammable and offers good arc resistance.Information provided by Pyrotek. |
|||
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC QC-7753 is a polyester engineered structural composite molding compound that is designed for applications requiring high strength, fire retardant properties, and resistance to elevated temperatures... |
|||
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8100 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and corrosion resistance. Form and Colors = Rolled Shee.. |
|||
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America EM 7302 Hardware Grade Epoxy Long fiberglass reinforced epoxy molding compound which features high strength and toughness for structural components. This compound is designed for applications requiring Mil-M-46069 certificatio.. |
|||
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Izod Impact, Notched | 16.0 J/cm | 30.0 ft-lb/in | |
Cosmic Plastics CP7312 Epoxy Molding Compound Data provided by the manufacturer. |