Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraton® G2705 GU (SEBS) Compound

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® G2705 GU (SEBS) Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton G2705 GU-N is an easy processing material designed for applications where FDA regulations are required. The material exhibits high resilience, low compression set, and good puncture resealing characteristics. It is also steam sterilizable. It is supplied from North America in the physical form identified: G2705 GU-N - supplied as a transparent pellet.Region: Asia Pacific, Europe, Japan, North America, and South AmericaApplications: Compounding and Personal HygieneInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.875 - 0.905 g/cc
0.875 - 0.905 g/cc
BAM 1014
Mechanical Properties Metric English Comments
Hardness, Shore A 52 - 62
52 - 62
Injection molded plaque at 205°C; BAM 1003
Tensile Strength 5.79 MPa
840 psi
Injection molded plaques, Die C, Machine Direction; ASTM D412
11.38 MPa
1651 psi
Injection molded plaques, Die C, Cross Direction; ASTM D412
Elongation at Break 650 %
650 %
Injection molded plaques, Die C, Machine Direction; ASTM D412
>= 800 %
>= 800 %
Injection molded plaques, Specimen did not break, Die C, Cross Direction; ASTM D412
100% Modulus 0.00162 GPa
0.235 ksi
Injection molded plaques, Die C, Cross Direction; ASTM D412
0.00193 GPa
0.280 ksi
Injection molded plaques, Die C, Machine Direction; ASTM D412
300% Modulus 0.00252 GPa
0.366 ksi
Injection molded plaques, Die C, Cross Direction; ASTM D412
0.00289 GPa
0.419 ksi
Injection molded plaques, Die C, Machine Direction; ASTM D412
Tear Strength 27.2 kN/m
155 pli
Injection molded plaques, Die C, Machine Direction; ASTM D624
29.8 kN/m
170 pli
Injection molded plaques, Die C, Cross Direction; ASTM D624
Compression Set 19 %

@Temperature 23.0 °C,
Time 79200 sec
19 %

@Temperature 73.4 °F,
Time 22.0 hour
Injection molded plaque; ASTM D395B
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified