Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Premix Thermoplastics PRE-ELEC® ESD 5000 Polyolefin Compatible Dissipative Masterbatch, IDP Additive

Category Polymer , Thermoplastic , Polyolefin, Film Grade , Polypropylene (PP)
Manufacturer Premix Thermoplastics Inc.
Trade Name PRE-ELEC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PRE-ELEC® ESD 5000 Polyolefin Compatible Dissipative Masterbatch, IDP Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PRE-ELEC® ESD 5000 is a polyolefin compatible dissipative masterbatch developed for PP injection moulded products. The active substance is an IDP (inherently dissipative polymer) and it gives a permanent dissipative property also at low humidity. The surface resistance level at 1x108 – 1x1012 ohms can be achieved at 8-20 % dosing level (EOS/ESD S11.11-1993, IEC 61340-5-1). The let down ratio of the masterbatch should be tested prior to its use with the polymer used in order to reach the desired dissipative level. PRE-ELEC® ESD 5000 can be used in clean room applications. The processing temperature should be less than 220 °C (430 ºF) and the material should be pre-dry before processing.Information from Premix OY
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 190 °C
11 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
Electrical Properties Metric English Comments
Surface Resistance 1.00e+8 - 1.00e+12 ohm
1.00e+8 - 1.00e+12 ohm
At 8-20% Dosing; ISO IEC 61340-5-1
Processing Properties Metric English Comments
Processing Temperature <= 220 °C
<= 428 °F
Drying Temperature 80.0 - 90.0 °C
176 - 194 °F
Pre-drying in a dehumidifier
Dry Time 3 - 4 hour
3 - 4 hour
Moisture Content <= 0.25 %
<= 0.25 %
when produced
Descriptive Properties Value Comments
Appearance Granule
Colour Yellowish