Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering S65E Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering S65E Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Red iron oxide filled, Phenyl Silicone Rubber, 65-75 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. Meets UK Ministry of Defence aerospace specification DTD818 Class M4 (now obsolescent and inactive for new design). ASTM & ISO designation = PVMQ.Applications: Excellent heat resistance plus ultra-low temperature flexibility. Used primarily for dry heat static seals. Low physical strength and poor abrasion resistance prevents dynamic sealing. Although silicone will swell in petroleum lubricants, this is not necessarily detrimental in static sealing applications.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
78
78
°IRHD, +8 change after 70 hours @ 200°C; ASTM D1415
Tensile Strength, Yield 7.238 MPa
1050 psi
-23% change after 70 hours @ 200°C; ASTM D412
9.40 MPa
1360 psi
ASTM D412
Elongation at Break 300 %
300 %
-40% change after 70 hours @ 200°C; ASTM D412
500 %
500 %
ASTM D412
Compression Set 30 %
30 %
70 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -120 °C
-184 °F
-120 °C
-184 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved